<?xml version="1.0" encoding="UTF-8"?><?xml-stylesheet type="text/xsl" href="static/style.xsl"?><OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd"><responseDate>2026-11-23T00:55:57Z</responseDate><request verb="GetRecord" identifier="oai:uwspace.uwaterloo.ca:10012/10452" metadataPrefix="dim">https://dspacemainprd01.lib.uwaterloo.ca/server/oai/request</request><GetRecord><record><header><identifier>oai:uwspace.uwaterloo.ca:10012/10452</identifier><datestamp>2025-03-26T23:36:01Z</datestamp><setSpec>com_10012_9900</setSpec><setSpec>com_10012_1</setSpec><setSpec>col_10012_9912</setSpec><setSpec>col_10012_6</setSpec></header><metadata><dim:dim xmlns:dim="http://www.dspace.org/xmlns/dspace/dim" xmlns:doc="http://www.lyncode.com/xoai" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.dspace.org/xmlns/dspace/dim http://www.dspace.org/schema/dim.xsd">
   <dim:field mdschema="dc" element="contributor" qualifier="advisor">Michael, Mayer</dim:field>
   <dim:field mdschema="dc" element="contributor" qualifier="author" authority="66dfd5d9-98df-409e-ad40-7690dd8ffed0" confidence="600">Laor, Ariel</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="accessioned">2016-05-09T19:46:30Z</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="available">2017-05-10T04:50:07Z</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="issued">2016-05-09</dim:field>
   <dim:field mdschema="dc" element="date" qualifier="submitted">2016-05-06</dim:field>
   <dim:field mdschema="dc" element="identifier" qualifier="uri">http://hdl.handle.net/10012/10452</dim:field>
   <dim:field mdschema="dc" element="description" qualifier="abstract" lang="en">Flip chip is an electronic packaging technology that is becoming more popular in first&#xd;
level electronic packaging as the need for high density electrical interconnects becomes more relevant.&#xd;
The parallel nature of flip chip and harsh thermomechanical treatment introduces stress to&#xd;
the microchip and substrate. This is primarily caused by the application of high forces and mismatch&#xd;
in the thermal coefficient of expansion among the materials in the system. Other noise factors&#xd;
like misalignment, parallelism mismatch, warpage, pillar height variation, and temperature&#xd;
variation can weaken the bonding process. Unlike wire bonding, there is a lack of tools available&#xd;
for quality assessment of the flip chip process in-situ locally at the interconnect sites. There are&#xd;
however some existing wire bonding sensor tools which can be modified to be useful for optimization&#xd;
of flip chip equipment and processes.&#xd;
&#xd;
A 4x3 mm CMOS chip is designed to record XYZ force and temperature profiles in-situ&#xd;
on a 2-dimensional surface during a simulated flip chip process. This was done as a low risk proof&#xd;
of concept to evaluate if the wire bonding tools can be adapted for a flip chip application. 95 μm&#xd;
square Al bond pads arranged in a square 8x8 array with 400 μm pitch have embedded piezoresistive&#xd;
force sensors and local top metal resistive temperature detectors. The chip is packaged with&#xd;
auxiliary wire bonds to deliver power and capture signals while operating under a bond head. Ball&#xd;
bumps 73 μm in diameter are deposited onto the sensor pads using 4N Au wire. Z sensors are calibrated&#xd;
using a modified automatic wire bonder. A normalized sensitivity of SN=1.39 mV/V/N is&#xd;
measured. Temperature sensors are calibrated at 50 °C using Kelvin probing yielding 186.94 Ω. A&#xd;
3x3 mm Si wafer with Al patterning is used as a dummy pressure plate for touchdowns on the&#xd;
sensor chip with an experimental setup advanced process bond head. Force and temperature signals&#xd;
are recorded locally at each bump. 80 N force with 200 °C temperature ramps ups are&#xd;
applied.&#xd;
&#xd;
Evidence of tilt and thermal expansion are detected. The prototype is demonstrated successfully&#xd;
and identified the most stressful stage of the bonding which occurred during thermal&#xd;
transients, i.e. during the short lived overshoot period of maximum stress in the force signals&#xd;
observed immediately after the application of heat to the system.</dim:field>
   <dim:field mdschema="dc" element="language" qualifier="iso" lang="en">en</dim:field>
   <dim:field mdschema="dc" element="publisher" lang="en">University of Waterloo</dim:field>
   <dim:field mdschema="dc" element="subject" lang="en">Flip Chip Electronic Packaging CMOS</dim:field>
   <dim:field mdschema="dc" element="title" lang="en">A Novel 8x8 CMOS Sensor Array for Thermal Compression Bonding with in-situ XYZ Force and Temperature Measurement</dim:field>
   <dim:field mdschema="dc" element="type" lang="en">Master Thesis</dim:field>
   <dim:field mdschema="dc" element="pending">false</dim:field>
   <dim:field mdschema="uws-etd" element="degree" qualifier="department" lang="en">Mechanical and Mechatronics Engineering</dim:field>
   <dim:field mdschema="uws-etd" element="degree" qualifier="discipline" lang="en">Mechanical Engineering</dim:field>
   <dim:field mdschema="uws-etd" element="degree" qualifier="grantor" lang="en">University of Waterloo</dim:field>
   <dim:field mdschema="uws-etd" element="degree" lang="en">Master of Applied Science</dim:field>
   <dim:field mdschema="uws-etd" element="embargo" qualifier="terms" lang="en">1 year</dim:field>
   <dim:field mdschema="uws" element="comment" qualifier="hidden" lang="en">fixed all issues as mentioned with TOC and page number&#xd;
&#xd;
My name is now displayed as Ariel.</dim:field>
   <dim:field mdschema="uws" element="contributor" qualifier="advisor">Michael, Mayer</dim:field>
   <dim:field mdschema="uws" element="contributor" qualifier="affiliation1" lang="en">Faculty of Applied Health Sciences</dim:field>
   <dim:field mdschema="uws" element="published" qualifier="city" lang="en">Waterloo</dim:field>
   <dim:field mdschema="uws" element="published" qualifier="country" lang="en">Canada</dim:field>
   <dim:field mdschema="uws" element="published" qualifier="province" lang="en">Ontario</dim:field>
   <dim:field mdschema="uws" element="typeOfResource" lang="en">Text</dim:field>
   <dim:field mdschema="uws" element="peerReviewStatus" lang="en">Unreviewed</dim:field>
   <dim:field mdschema="uws" element="scholarLevel" lang="en">Graduate</dim:field>
   <dim:field mdschema="others" element="access-status">open.access</dim:field>
</dim:dim>
</metadata></record></GetRecord></OAI-PMH>